    SAE USCAR5-5

    AVOIDANCE OF HYDROGEN EMBRITTLEMENT OF STEEL FASTENERS AND OTHER HARDENED OR SPRING STEEL PARTS FROM SURFACE COATING PROCESSES
    • 발행일 : 2019-02-27
    • 발행기관 : SAE
    즐겨찾기 장바구니 담기
    닫기

    상품이 장바구니에 담겼습니다.

    장바구니로 이동
    • [영어]PDF 119,300원

    • [영어]PRINT 119,300원

상세정보

분야
적용범위

This standard outlines the conditions that enhance the risk of hydrogen embrittlement of steel and defines the relief procedures required to minimize the risk of hydrogen embrittlement. It is intended to control the process.

Hydrogen embrittlement of steel, which can cause brittle fractures under stress, occurs as a result of the absorption of hydrogen during cleaning, phosphate coating and plating processes. The susceptibility to hydrogen embrittlement increases with increasing stress (internal or externally applied stress) and increasing material strength.

Hardness readings in this specification are in Vickers scale. SAE J417 should be referred to for conversion to other scales.

국제분류(ICS)코드
페이지수 5
Edition

이력정보

No. 표준번호 표준명 발행일 상태
1 SAE USCAR5-5상세보기 AVOIDANCE OF HYDROGEN EMBRITTLEMENT OF STEEL FASTENERS AND OTHER HARDENED OR SPRING STEEL PARTS FROM SURFACE COATING PROCESSES 2019-02-27 표준

제공형태 닫기

  • PDF :

    직접 파일 다운로드 및 인쇄(마이페이지 확인)
  • 보안PDF :

    직접 파일 다운로드 및 인쇄(마이페이지 확인)* 단, 파일이동 및 복사 불가, 1회 다운로드 및 인쇄가능
  • PRINT :

    인쇄본 우편발송, 2~3일 소요(PDF파일 미제공)
  • BOOK :

    인쇄본 우편발송, 2~3일 소요(PDF파일 미제공)
  • ZIP :

    압축파일형태로 제공 (PDF, HTML, TXT, XLS 등으로 구성), 직접 파일 다운로드(마이페이지 확인)
  • CD/DVD :

    직접 파일 다운로드 및 인쇄(마이페이지 확인)
  • DB :

    별도 정보 제공
  • HARDCOPY :

    해외 배송 상품, 최대 3주 소요
  • 바인더 :

    바인더 우편발송, 2~3일 소요
  • 온라인구독 :

    WEB 접속 후 실시간 열람, 출력(1년간)